DES was immobilized on ceria NPs by making use of ethanol through a solvent evaporation strategy and filler for that MMMs was attained. Polysulfone was employed as support content to maintain the toughness of your membrane matrix since it is easy to system, mechanically sturdy, and thermally and chemically steady. Ultimately, mixed matrix membranes